Titanium plate is a flat-rolled titanium product supplied above the thickness at which the material is classified as sheet, produced by hot rolling followed by controlled annealing. Titanium itself is a light, strong and highly corrosion-resistant metal: its low density makes it attractive wherever weight is critical, its tensile strength to density ratio is the highest of the common structural metals, and its biocompatibility means the human body tolerates it far better than most other engineering materials. Those three properties together explain why the same product family serves aircraft structures, surgical implants and chemical plant equipment.
The distinction between plate and sheet is a thickness convention rather than a difference in alloy. Under ASTM B265, flat-rolled titanium is classified as plate from 4.76 mm (0.1875 in) upward, while thinner material is supplied as sheet or strip. In commercial practice buyers should always state the thickness, width, length and tolerance class explicitly, because the same grade and heat can be supplied in either form and because plate is normally supplied with as-rolled or annealed surfaces rather than the pickled finish typical of thin sheet. Sheet is the usual choice for cladding, liners and formed components, while plate is specified where the section must carry structural load, be machined into a flange or tube sheet, or resist abrasive process conditions.
| Grade 1 | O <= 0.18%, Fe <= 0.20% | ||
| Grade 2 | O <= 0.25%, Fe <= 0.30% | The general-purpose corrosion-resistant grade | |
| Grade 3 | O <= 0.35%, Fe <= 0.30% | ||
| Grade 4 | O <= 0.40%, Fe <= 0.50% | ||
| Grade 5 | Alpha-beta alloy | Al 5.5–6.75%, V 3.5–4.5% | High-strength structural and aerospace grade |
| Grade 7 | Pd 0.12–0.25% | ||
| Grade 12 | Ni 0.6–0.9%, Mo 0.2–0.4% |
The commercially pure grades are distinguished mainly by their oxygen and iron content, and it is the oxygen level that drives strength: raising oxygen from the Grade 1 level to the Grade 4 level increases strength appreciably while reducing ductility. Grade 5 is the workhorse structural alloy, and Grades 7 and 12 exist specifically to solve corrosion problems in reducing environments where unalloyed titanium would not survive.
The values below are the minimum requirements commonly applied to annealed titanium plate under ASTM B265. They are expressed as the tensile strength, the 0.2% offset yield strength and the elongation in 50 mm.
| Yield strength, 0.2% offset (min) | |||
|---|---|---|---|
| Grade 1 | 240 MPa | 138 MPa | 24% |
| Grade 2 | 345 MPa | 275 MPa | 20% |
| Grade 3 | 450 MPa | 380 MPa | 18% |
| Grade 4 | 550 MPa | 483 MPa | 15% |
| Grade 5 | 895 MPa | 828 MPa | 10% |
| Grade 7 | 345 MPa | 275 MPa | 20% |
| Grade 12 | 483 MPa | 345 MPa | 18% |
Alongside the room-temperature values, titanium plate is normally specified with a maximum oxygen, nitrogen, hydrogen and iron content, because interstitial elements control both strength and toughness. Grade 5 plate also carries an aluminium and vanadium range rather than a maximum, and both the aluminium and the vanadium content must fall inside the band for the alloy to meet its property targets.
structural plate, fittings and brackets where high strength and low weight are combined; Grade 5 is the default choice.
implant components and surgical instruments, where biocompatibility and corrosion resistance in body fluid are essential.
pressure vessel plate, heat exchanger tube sheets, column internals and piping components in chloride and oxidising acid service.
condenser plate and seawater-exposed structures, using Grades 2, 7 and 12 according to the severity of the environment.
heat exchangers, anode baskets, architectural panels and precision equipment frames, where the metal can be polished to a lustrous finish that keeps its appearance over time.
Titanium plate is normally supplied in the annealed condition, which gives a stable microstructure suitable for forming and machining. Cold forming requires more force and more springback allowance than mild steel, and hot forming must respect the limits in the applicable specification to avoid contaminating the surface. Titanium must never be welded or heated in contact with iron or copper contamination, because absorbed iron embrittles the weld; dedicated stainless steel brushes, separate cutting tools and controlled cleaning of the joint area are standard workshop practice. Machining is performed with sharp tooling, low cutting speeds, generous coolant and heavy feed rates to avoid work hardening at the surface. Because titanium is a poor conductor of heat, heat input during welding should be controlled and the interpass temperature limited to protect the mechanical properties of the plate.
Titanium plate is flat-rolled titanium supplied above the thickness at which the product is called sheet; under ASTM B265 that threshold is 4.76 mm, and plate is produced by hot rolling followed by annealing.
Only the thickness convention. Sheet is thinner than 4.76 mm and is used for cladding, liners and formed parts, while plate is supplied from 4.76 mm upward for structural, machined and pressure-retaining components.
Grade 2 is the general-purpose corrosion-resistant grade, Grade 5 (Ti-6Al-4V) is used where strength and weight dominate, and Grades 7 and 12 are selected for reducing acid and chloride service.
Minimum tensile strength ranges from 240 MPa for Grade 1 to 895 MPa for Grade 5, with Grade 2 at 345 MPa and Grade 12 at 483 MPa.
Because the metal is biocompatible, resists body fluid corrosion and has a low density, which allows implants and surgical instruments to be strong while remaining light.
Iron and copper contamination during heating or welding, indiscriminate tool sharing, and excessive heat input, all of which can embrittle the plate or degrade its properties.